Abstract: Different thermal treatments were performed to produce a protective coating on the surface of SiC particles in order to allow their incorporation in a glass matrix. These oxidation treatments were carried out in air at different temperatures ranging from 800 degrees C to 1500 degrees C and different times at 1200 degrees C (10 min-48 h). The oxidation kinetics followed the Deal-Grove model and the thickness of the protective coating increased with temperature and SiC particle size. Protected SiC particles with different particle sizes were incorporated in a borosilicate glass. With small particles sizes foam glasses were obtained, whereas particles with higher grain size, i.e., higher coating thickness, were stable in the glass matrix and a smooth glass was obtained. | |
Internacional
|
Si |
JCR del ISI
|
Si |
Título de la revista
|
J EUR CERAM SOC |
ISSN
|
0955-2219 |
Factor de impacto JCR
|
1,562 |
Información de impacto
|
|
Volumen
|
27 |
DOI
|
|
Número de revista
|
1 |
Desde la página
|
861 |
Hasta la página
|
865 |
Mes
|
SIN MES |
Ranking
|